manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

The Pressure Electroslag Remelting Process (PESR)

1 What is PESR?

The pressure electroslag remelting process is a recent advancement and allows for the manufacture of new high nitrogen alloys with unique properties under pressures of several atmospheres.
Much higher levels of nitrogen can be achieved due to the pressure applied above the slag which can be increased significantly above normal atmospheric pressure levels.

2 What is ESR?

The ESR is the metallurgic process for the production of steel with high purity and a controlled solidified and respectively faultless structure. It is well known as a refining method used mainly in the steel and superalloy industry. The main goal of this process is the inclusion, removal, desulphurization and the adjustment of a uniform microstructure. The fundamentals of this process are described elsewhere and are not further outlined in this paper.

3 How ESR works?

Many alloys contain elements like aluminum and titanium which, when heated, react with oxygen to form oxides. Oxides are detrimental to premium quality melted alloys. Premium grade alloys, such as those required by the aerospace, energy, medical and automotive industries, can be protected from the atmosphere and residuals by melting inside a vacuum container. This approach gives the metals producer more control over alloy chemistry. The result is a cleaner, more uniform product with the superior properties required for critical service applications.

On the other hand, the investments in state-of-the-art technology such as Pressure Electro Slag Remelting (PESR), Vacuum Induction Melting (VIM) and Vacuum Arc Remelting (VAR) are the result of research showing a real need for a new generation of steels.

Electroslag Remelting (ESR) is a secondary refining process used to further refine many alloys. As a feedstock it uses consumable electrodes produced either by VIM or conventional air melting. Conventional ESR improves the microstructure and cleanliness of the VIM, or arc melted alloy, by removing inclusions as the metal passes through the slag and controlling the solidification rate in the refined metal ingot to minimize chemical segregation. Melting through the slag permits very close compositional control.

4 How PESR works?

A more recent advancement is Pressurized ESR (P-ESR) furnaces, which have the ability to melt alloys under nitrogen pressures of several atmospheres and produce very high nitrogen steel compositions that cannot be achieved via standard air melting techniques. This capability allows the manufacture of new and novel high-nitrogen alloys with unique mechanical properties.

Pressure ESR (P-ESR) is an even more advanced process than standard ESR. With pressure ESR the metal is melted under elevated nitrogen pressure, permitting the production of alloys with high levels of nitrogen. For P-ESR, the standard ESR crucible is enclosed and becomes a pressure vessel melt chamber. With this design, the pressure above the slag can be increased to levels that are significantly above normal atmospheric pressure levels, enabling much higher levels of nitrogen to be achieved. The P-ESR furnace can also melt at atmospheric pressure, in an air atmosphere or with an inert gas cover of argon over the slag. Having an inert gas cover over the slag enables enhanced compositional control of reactive elements, such as aluminum and titanium, during melting. The high-nitrogen compositions from the P-ESR process cannot be achieved through either conventional ESR or VAR melting techniques.

electroslag remelting

We can supply ESR and PESR material of h13 forged

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x