manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

Stainless Steel Wires

nickel alloy spring wire

Stainless Steel Wires

 

Stainless Steel Wires are widely used in chemical industry, paper-making, mechanic industry & woven netting etc. They can also be used to make filters. Stainless Steel Wires used for the cold heading quality are fit for fasteners such as nut bolt, nut & threaded rod, self tapping screw, etc. They are widely used in household electric in appliance & mechanic-electronic industry etc.

 

As a professional manufacturer, we can provide different size of Wire with good quality and reasonable price. We specialise in the supply and processing of stainless steel wire.­ Our wire is of the highest quality produced to a wide range of diameters and tensile strengths to suit customer appli­cations. we can cut to length, change the shape of the wire or process to smaller coils.We can also produce unique sizes, grades or tensile strengths to order. We work closely with our customers so that material can be available for immediate delivery. This means our customers’ are able to reduce their own inventory levels, saving money and space.

 

  1. Competitive price and quality from our own factory
  2. Approved by ISO9001, CE, SGS every year
  3. Best service with 24 hour`s reply
  4. Flexible payment with T/T,L/C , paypal, kunlun bank, etc
  5. Smooth production ability(50000tons/month)
  6. Quick delivery and standard exporting package
  7. OEM/ODM

 

Specifications:

(1) Grade: 201, 202, 302, 301, 303, 304, 304L, 305, 316, 316L, ,316Ti, 310S, 317, 321, 410, 416, 420, 430 etc

(2) Standard: ASTM A240,GB/T3280-2007,JIS4304-2005,ASTM A167,EN10088-2-2005,etc

(3) Diameter: 0.01-30mm

(4) Surface: 2B,2D,BA,NO.1,NO.4,NO.8,8K,mirror,checkered,embossed,hair line,sand blast,etching,brush,etc

(5) Tensile strength: soft (650-850N/mm2) and hard (around 2000N/mm2)

(6) Packing: in Coil or in Spool then in Carton or as customers’ request

(7) Quality assurance: Mill Test Certificate is supplied with shipment, third Party Inspection is acceptable

 

Product Application:

Uses:It is widely used in chemical industry, paper-making, mechanic industry & woven netting etc. They can also be used to make filters. Stainless Steel Wires used for the cold heading quality are fit for fasteners such as nut bolt, nut & threaded rod, self tapping screw, etc. They are widely used in household electric in appliance & mechanic-electronic industry etc.

 

Why Choose Us :

  1. You can get the perfect material according to your requirement at the least possible price.
  2. We also offer Reworks, FOB, CFR, CIF, and door to door delivery prices. We suggest you to do deal for shipping which will be quite economical.
  3. The materials we provide are completely verifiable, right from raw material test certificate to the final dimensional statement.(Reports will show on requirement)
  4. guarantee to give a response within 24hours(usually in the same hour)
  5. You can get stock alternatives, mill deliveries with minimizing manufacturing time.
  6. We are fully dedicated to our customers. If it will not possible to meet your requirements after examining all options, we will not mislead you by making false promises which will create good customer relations.

 

Quality Assurance (including both Destructive and Non-Destructive) :

  1. Visual Dimension Test
  2. Mechanical examining like tensile, Elongation and reduction of area.
  3. Impact analysis
  4. Chemical examination analysis
  5. Hardness test
  6. Pitting protection test
  7. Penetrant Test
  8. Intergranular Corrosion Testing
  9. Roughness Testing
  10. Metallography Experimental Test

 

Chemical Component:

Type AISI C Max % Mn Max % P Max S Max Si Max Cr Ni Mo
201 0.15 5.50-7.50 0.06 0.03 1 16.000-18.00 0.5
202 0.15 7.50-10.00 0.06 0.03 1 17.00-19.00 3.-0-5.00
204Cu 0.08 6.5-8.5 0.06 0.03 2 16.0-17.0 1.5-3.0
302 0.15 2 0.045 0.03 1 17.00-19.00 8.00-10.00
302HQ 0.03 2 0.045 0.02 1 17.00-19.00 9.00-10.00
304Cu
304HC 0.04 0.80-1.70 0.04 0.015 0.3-0.6 18-19 8.5-9.5
303 0.07 2 0.045 0.25 Min 1 17-19 8.0-10.0 0.6
304 0.08 2 0.045 0.03 1 18.00-20.00 8.0-10.50
304L 0.03 2 0.045 0.03 1 18.00-20.00 8.00-12.00
310S 0.055 1.5 0.04 0.005 0.7 25.0-28.0 19-22
314 0.25 2 0.045 0.03 1.50-3.00 23.00-26.00 19.00-22.00
316 0.06 2 0.045 0.03 1 16.00-18.00 10.00-14.00 2.00-3.00
316L 0.03 2 0.045 0.03 1 16.00-18.00 10.00-14.00 2.00-3.00
316Ti 0.08 2 0.045 0.03 0.75 16.00-18.00 10.00-14.00 2.00-3.00
347 0.08 2 0.045 0.03 1 17.00-19.00 9.00-13.00
321 0.06 2 0.045 0.01 .40-.60 17-19.00 9.4-9.6
308 0.08 2 0.045 0.03 1 17-19 9.5-13.0
308L 0.025 1.50/2.00 0.025 0.02 0.5 19.0/21.0 9.5/11.0
309 0.08 1.50/2.50 0.02 0.015 0.5 23.0/25.0 20.0/14.0
309L 0.025 1.50/2.50 0.02 0.015 0.5 23.0/25.0 12.0/14.0
316L 0.02 1.50/2.00 0.02 0.02 0.5 18.0/20.0 12.00-14.00 2.00-3.00
430L 0.03 1 0.04 0.03 1 16.00-18.00
434 0.08 1 0.04 0.03 1 16.00-18.00 0.90-1.40

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x