S32050 Super Austenitic Stainless Steel

S32050 Super Austenitic Stainless Steel

Product Description

UNS S32050 is a high corrosion resistant super austenitic stainless steel characterized by its elevated content of nickel (20-23%), chromium (22-24%), and molybdenum (6.0-6.8%). This premium alloy is designed to withstand severe corrosion environments, particularly those involving high-temperature seawater and concentrated chloride solutions. It offers an excellent balance of corrosion resistance comparable to nickel alloys and pure titanium, but with greater economic efficiency. At FUSHUN METAL, we supply UNS S32050 in various forms to meet diverse industrial requirements for applications demanding exceptional corrosion resistance in challenging environments.

Applications

UNS S32050 super austenitic stainless steel is specifically designed for applications that demand exceptional corrosion resistance in aggressive environments:

  • Seawater Environments:Seawater desalination systems, seawater heat exchangers, condenser tubes
  • High Concentration Chloride Environments:Pulp and paper plants, various types of bleaching systems
  • Chemical Processing:Equipment handling aggressive chemicals, storage tanks, and reaction vessels
  • Oil & Gas:Offshore platforms, subsea equipment, and components exposed to corrosive conditions

Standards

UNS S32050 conforms to the following international standards:

  • American Standard:ASTM A240 (UNS S32050)
  • European Standard:Comparable to EN 1.4466 (slightly different composition)
  • Japanese Standard:Proprietary high-performance stainless steel grade

Chemical Composition

Element C Si Mn P S Ni Cr Mo Cu N
(UNS S32050) ≤0.030 ≤1.00 ≤1.50 ≤0.035 ≤0.020 20.0-23.0 22.0-24.0 6.0-6.8 ≤0.40 0.21-0.32

Mechanical Properties

UNS S32050 offers exceptional mechanical properties that make it suitable for demanding applications:

Property Value
0.2% Proof Stress ≥330 MPa
Tensile Strength ≥675 MPa
Elongation ≥40%
Hardness ≤250 HB

Critical Pitting Corrosion Temperature (CPT): 95°C (ASTM G48 Method C)

Critical Crevice Corrosion Temperature (CCT): 45°C (ASTM G48 Method D)

Available Dimensions

FUSHUN METAL provides UNS S32050 in the following dimensions:

Form Thickness (mm) Width (mm) Length (mm)
Plate 3.0 – 100.0 1000 – 2500 2000 – 12000
Sheet 0.5 – 3.0 1000 – 1500 2000 – 6000
Strip 0.1 – 0.5 10 – 600 Coil
Bar Diameter 5-600mm

Why Choose FUSHUN METAL for UNS S32050

When it comes to super austenitic stainless steel like UNS S32050, quality and reliability are paramount. Here’s why customers choose us:

  • Superior Quality Control:Our rigorous testing ensures that every sheet, plate, and strip of UNS S32050 meets or exceeds international standards
  • Technical Expertise:Our metallurgists provide expert guidance on material selection and application
  • Competitive Pricing:Direct sourcing and efficient operations allow us to offer premium materials at competitive prices
  • Custom Solutions:We can provide UNS S32050 with custom dimensions and finishes to meet your specific requirements
  • Global Delivery:Reliable shipping to destinations worldwide with comprehensive documentation

For specialized applications requiring exceptional corrosion resistance in severe environments, UNS S32050 from FUSHUN METAL offers the optimal balance of performance and value. Contact us today to discuss your requirements and request a quotation for this premium super austenitic stainless steel.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x