We produce P650 HS non-mag material Steel Bars and Non Magnetic Hollow Bars.

 

1. CHEMICAL COMPOSITION

P650 HS is a special nonmagnetic, austenitic Mn-Cr-Mo-N-steel with a high pitting corrosion resistance , specifically developed for oilfield applications.

C Mn Cr Mo N Ni
max. 0,06 19,50 – 20,50 18,00 – 19,00 1,70 – 2,00 0,55 – 0,65 3,00 – 4,50

 

2. MECHANICAL PROPERTIES

Following mechanical properties (tested at room temperature) are achieved by a special cold-working process over the full length of the collar:

TEXT OD KSI N/MM
Yield Strength (min.) 0,2%-offset method: OD up to 9 1/4“ 180 ksi 1242 N/mm²
OD 9 1/2“ and larger 170 ksi 1173 N/mm²
Tensile Strength (min.): 185 ksi 1277 N/mm²
Elongation (min.): 12% 12%
Reduction of area (min.): 50% 50%
Impact energy (min.): 80 ft.lb 110 J
Endurance Strength / N=10⁵ (min.): 80 ksi 550 N/mm²
Hardness Brinell: (min.): 330-450 HB 330-450 HB

 

3. MAGNETIC PROPERTIES

Relative permeability: ≤ 1,005.

 

4. CORROSION RESISTANCE

  • Transgranular SCC:Prevented by special surface treatments (Hammer peening, roller burnishing, shot peening).
  • Intergranular SCC:The occurrence of material sensitization is prevented by quenching after warm forging. Each collar is tested according to ASTM A 262, Pract.A and E, last edition.
  • Pitting Corrosion:Due to a high chromium-, molybdenum- and nitrogen contents a high resistance to pitting corrosion is given.

 

5. NON-DESTRUCTIVE TESTING

  • Magnetic inspection:Drill collars are 100% tested by a proprietary probe-testing process. Magnetic permeability of each collar is certified with the printout of probe-testing.
  • Ultrasonic inspection: Each collar is ultrasonically inspected over 100% of the volume according to ASTM E 114, last edition as a minimum level.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x