manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

Nickel Alloy Spring Wire

Nickel Alloy Spring Wire

nickel alloy spring wire

nickel alloy spring wire

Fushun produces a full line of nickel alloy spring wire, produced for the performance required in aerospace, automotive, oil & gas, and general industrial applications. Wire is available in a range of alloys and packaging options.

 

With over 35 years of industry expertise, Fushun has the industry knowledge and resources to find you the metal products that you need for your specific industry applications. We are in stock and ready to quickly deliver hard-to-find metals. Our ISO 9001-certified metal supply is one of the most comprehensive selections on the market. We provide timely customer support and quick delivery on all quantities of our in stock products.

 

Contact us for more information regarding our nickel alloy manufacturing and distribution options.  Fushun is your trusted nickel alloy supplier for all types of Nickel alloy material.

 

1.Why choose our nickel alloy spring wire?

Our wire exhibits excellent coiling ability at high speeds and often requires no additional lubricant. This results in less stress on coiling equipment, preserving equipment life, minimizing downtime and maximizing throughput and profits. If additional lubrication is required, we offer several performance coating options.

Our technical and metallurgical team talk through spring manufacturers’ technical requirements, material application and help solve potential manufacturing situations around the need for corrosion resistant and high temperature performing wire.

We understand exactly what the spring maker needs for precision coiling and supply exactly how they want it, guaranteeing consistency in temper and a dead cast whether that is wire in coils with a soap coating or clean on spools. There is even the option of straight bars.

 

2.What is nickel alloy spring wire?

Nickel-based alloys are especially useful spring materials. Their chemical composition makes them highly corrosion resistant, and they perform well in extreme high and low temperatures. Most nickel alloys are nonmagnetic, an important property for devices such as gyroscopes, chronoscopes, and indicating instruments. Nickel alloys exhibit high electrical resistance, and therefore should not be used as electrical conductors.

Nickel alloys for use in harsher environments include MP35N, Inconel® 718, Inconel® 600, and Alloy X750. Tensile Strengths range from gull soft to full hard “spring temper”. Performance is tested on every lot of material to ensure we meet your requirements, and full reports are available upon request.

 

3.Where nickel alloy spring wire use?

As specialists in High Performance nickel alloys, one of our largest and most diverse markets globally is the spring manufacturing industry. They produce compression springs, tension springs, torsion springs and formed parts from our wire to perform in critically demanding places like aircraft engines, nuclear installations, valves and deep down oil wells – where other wire fails to perform.

 

4.Size of nickel alloy spring wire

What we do really well is producing any wire size between 0.025mm (.001”) to 21mm (.827”) to precise tolerances – typically delivered within 3 weeks. The spring industry today is demanding more wire that is certified to an increasing number of specifications, or produced to the customer’s own special mechanical properties, which we also support very well. Other sizes and alloys are available upon request.

 

5.Grades and Standard

Material (Nickel) Modulus of Elasticity Magnetic Corosion Fatigue T.P/T.S.** Maximum Safe Temp. Corrosion Resistance (General) Spring Temp.Range (KSI)
Torsion 10’  Tension 10’ High  Low
M400 10 10 Varies Good 450 ℉ -320 ℉ Good 145/180
K-500 10 10 No Good 38/42 500 ℉ -423℉ Good 145/195
600 11 11 No Good 40/45 750℉ -423℉ Good 170/230
601 11.5 11.5 No Good Good 120/205
625 11 11 No Excellent 700℉ -423℉ Excellent
718* 11 11 No Good 1200℉ -423℉ Good 210/250
X750 11 11 No Good 40/45 1200℉ -453℉ Good 190/230
800 11 11 No Good Good 140/175
805 9 9 Slight Good Good 150/190
825 10 10 No Good Good
*NS902 9.5 9.5 Slight Fair Fair 140/160
H C-276 11.4 11.4 No Excellent Excellent

 

6.Recommended Thermal Treatments

Alloy Stress Equalizing
Temp °F  Time (hrs)*
Age Hardening
Temp (°F) Time (hrs)*
Maximum Safe Operatin Temperature (°F)
alloy 400 575-650     1/2-1 Not Possible 450
alloy K-500 575          1/2-1 1,000               4-10 500
Permanickel 300 575          1/2-1 900               8 600
alloy 600 800-900     1/2-1 Not Possible 750
alloy 625 Not recommended Not Possible 700
alloy X750 Spring temper 875        3 1,200                4 700
alloy X750 (>0.025” diam.) w1 Temper (15% cold work) Not recommended 1,350                16 1,000
alloy X750 (Annealed) Spring temper (<0.025” diam.) Not recommended 1,350               16 1,200
alloy X750 Spring temper Age hardening also relieves stress Solution treat at 2,100 for 2hrs high temp age at for 1,550 24hrs regular age at 1,300 for 20 hrs 1,200
alloy 718 Spring temper Age hardening also relieves stress 1,325 for 8 hrs, 1,150 for 8 hrs 1,000
alloy 718 wl Temper (15% cold work) Not recommended 1,800fori hr, 1,320for8hrs furnace cool to 1,150 for 8 hrs 1,200
Ni-Span C 902 750          1.4 1,100-1,350          4-5
alloy 805 (Temperature compensating) 750        1/2 Not Possible
alloy 825 800          1 Not Possible

Quality & Testing

Fushun supply Certification with all shipments, containing full chemical analysis and also mechanical test results if requested.

 

All incoming material is visually inspected and PMI (Positive Material Identification) tested before processing begins and all our production material is checked during each stage of processing.

 

All incoming orders are produced to the individual customer specification, some of which may involve processing sample batches for testing prior to full production.

 

Final Inspection carried out on all finished material to include:

Visual inspection

Dimensional checks

PMI (Positive Material Identification)

Mechanical tests

 

Nickel Alloy Material Available Formats

Fushun offers pure Nickel alloy materials in a variety of forms, including:

Seamless & welded pipe

Seamless & welded tube

Bar

Wire

Sheet

Plate

Forgings

Pipe fittings

Flanges

Weld Rod

 

Nickel Alloy Supply Quantities for Single Items or Full Bills

At Fushun, we can supply single items or full bills of nickel alloy materials for most any project. No inquiry is too small. We offer quick responses to customer inquiries and specialize in the rapid delivery of both large and small quantities of nickel alloy products.

 

Contact Fushun for Nickel Alloy Materials Today

Contact us for more information regarding our nickel alloy material options, or request a quote for further pricing details today. Fushun is your trusted nickel alloy supplier and manufacturer of premium nickel alloy materials.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x