manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

Martensitic Stainless Steel Strip & Plate For Cutting knives

Martensitic Stainless Steel Strip & Plate For Cutting knives

Martensitic Stainless Steel Strip & Plate For Cutting knives

Martensitic Stainless Steel Strip & Plate For Cutting knives

FUSHUN SPECIAL STEEL is proud to present our premium line of Heat Treated Tempered Carbon Steel and Martensitic Stainless Steel Plates. These high-quality materials are engineered to meet the demanding requirements of various industrial applications.

 

At FUSHUN SPECIAL STEEL, we understand the critical importance of material quality in the performance of cutting tools, industrial equipment, and medical instruments. Our heat-treated tempered carbon steel and martensitic stainless steel plates are manufactured using advanced metallurgical processes to ensure optimal microstructure and properties.

 

Product Applications:

  1. Hard alloys, ceramic alloys, and PCD circular saw blade substrates
  2. Various industrial, household, and food processing tools
  3. Medical instruments

 

Key Product Features:

– Excellent flatness

– Uniform hardness distribution

– Resistant to deformation

– Versatile properties to meet different cutting and wear resistance requirements

 

Some Specifications

1.15 * 610 * 1830

1.30 * 610 * 1830

1.65 * 510 * 2050

1.85 * 620 * 1860

2.24 * 620 * 1830

2.55 * 410 * 2050

2.25 * 220 * 1320

3.00 * 250 * 1250

Chemical Component

Steel grade C Si Mn P S Cr Mo V N
SUS410 ≦0.15 ≦1.00 ≦1.00 ≦0.040 ≦0.030 11.50 – 13.50
SUS420J1 0.16 – 0.25 ≦1.00 ≦1.00 ≦0.040 ≦0.030 12.00 – 14.00
SUS420J2 0.26 – 0.40 ≦1.00 ≦1.00 ≦0.040 ≦0.015 12.00 – 14.00
EN1.4116 0.45 – 0.55 ≦1.00 ≦1.00 ≦0.040 ≦0.030 14.00 – 15.00 0.50 – 0.80 0.10 – 0.20
SUS420H 0.60 – 0.65 ≦0.6 ≦0.6 ≦0.040 ≦0.030 12.50 – 14.00 ≦0.06

 

Mechanical Properties

Steel grade 0.2%Yield strength Tensile strength Elongation Hardness
N/mm² N/mm² (%) Hv HRC
SUS410 ≧205 ≧440 ≧20 ≦93 ≦210
SUS420J1 ≧225 ≧520 ≧18 ≦93 ≦234
SUS420J2 ≧225 ≧540 ≧18 ≦99 ≦247
EN1.4116 ≦850 ≧12 ≦280
SUS420H ≧195 ≧410 ≧18 ≦90 ≦210

 

Whether you’re producing circular saw blades, specialized cutting tools, food processing equipment, or medical devices, our steel plates provide the perfect balance of hardness, toughness, and machinability. The variety of grades and dimensions available ensures that we can meet your specific requirements.

 

Contact FUSHUN SPECIAL STEEL today to discuss how our heat-treated tempered carbon steel and martensitic stainless steel plates can enhance the quality and performance of your products. Let us be your partner in achieving excellence in cutting-edge technology and precision manufacturing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x