manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

Incoloy 825 UNS N08825 2.4858 NiCr21Mo Nickel Alloy

Incoloy 825 UNS N08825 2.4858 NiCr21Mo Nickel Alloy

Incoloy 825 UNS N08825 2.4858 NiCr21Mo Nickel Alloy

Incoloy 825 UNS N08825 2.4858 NiCr21Mo Nickel Alloy

With over 35 years of industry expertise, Fushun has the industry knowledge and resources to find you the metal products that you need for your specific industry applications. We are in stock and ready to quickly deliver hard-to-find metals. Our ISO 9001-certified metal supply is one of the most comprehensive selections on the market. We provide timely customer support and quick delivery on all quantities of our in stock products.

 

Contact us for more information regarding our nickel alloy manufacturing and distribution options.  Fushun is your trusted nickel alloy supplier for all types of Nickel alloy material.

Introduce

UNS N08825 Incoloy 825 is a nickel-iron-chromium alloy that contains small amounts of titanium, copper, and molybdenum. Incoloy® 825’s chemical composition provides great resistance to many corrosive environments, such as pitting, crevice corrosion, intergranular corrosion, and stress- corrosion cracking. Incoloy 825 nickel alloy has good mechanical properties from moderate to high temperatures, with a hot- working range of 1600 to 2150º F. Alloy 825 also maintains good weldability for all conventional processes.

Applications

Nickel alloy UNS N08825 has many different industrial applications, some of which include: Propeller shafts, Phosphoric acid evaporators, Tank trucks, Hot vessels for food, water, sea water, Sulphuric acid piping and vessels, Marine exhaust systems

Standard

Rod, Bar, Wire and Forging Stock: BS 3076NA16, ASTM B 425, ASTM B 564, ASME SB 425, ASME SB 564, ASME Code Case N-572, DIN 17752, DIN 17753, DIN 17754, VdTÜV 432, ISO 9723, ISO 9724, ISO 9725.

Plate, Sheet and Strip: BS 3072NA16, BS 3073NA16, ASTM B 424, ASTM B 906, ASME SB 424, ASME SB 906, DIN 17750, VdTÜV 432, ISO 6208.

Pipe and Tube: BS 3074NA16, ASTM B 163, ASTM B 423, ASTM B 704, ASTM B 705, ASTM B 751, ASTM B 775, ASTM B 829, ASME SB 163, ASME SB 423, ASME SB 704, ASME SB 705, ASME SB 751, ASME SB 775, ASME SB 829, ASME Code Case 1936, DIN 17751, VdTÜV 432, ISO 6207.

Others: ASTM B 366, ASME SB 366, DIN 17744

Chemical Composition

Ni Fe Cr Mb Cu Ti C Mn S Si Al
38.0-46.0 22.0 min 19.5-23.5 2.5-3.5 1.5-3.0 .6-1.2 0.05 max 1.0 max 0.03 max 0.5 max 0.2 max

Mechanical Properties

Form Condition Ultimate

Tensile

Strength,

ksi (MPa)

Yield

Strength

at 0.2%

offset,

ksi (MPa)

Elongation

in 2″

or 4D, percent

Sheet

Plate

Strip, Bar

Annealed

Annealed

Annealed

100 (689)

95 (655)

85 (590)a

55 (379)

45 (310)

35 (240)a

39

44

30a

Weldability

Alloy 825 can be readily welded by the shielded metal-arc process using alloy welding electrode 135, the gas shielded arc processes using alloy filler metal 65, and the resistance welding processes. The alloy requires no postweld heat treatment. The corrosion resistance of deposited weld metal from both covered electrode and bare wire is equivalent to that of the parent metal.

Heat Treatment

Incoloy 825 is stabilise annealed at 940°C. The softest structure is obtained at 980°C. Sections heavier than sheet, strip and wire should be quenched to avoid sensitisation.

Corrosion Resistance

The outstanding property of Incoloy 825 is its corrosion resistance. In reducing & oxidising conditions, Incoloy 825 resists general corrosion, pitting & crevice corrosion, intergranular corrosion and stress corrosion cracking. It is particularly useful in sulphuric & phosphoric acids, sulphur containing flue gases, sour gas and oil wells and sea water.

Machinability

Incoloy 825 is classed as a ‘C’ alloy, and is reasonably easy to machine.

Quality & Testing

Fushun supply Certification with all shipments, containing full chemical analysis and also mechanical test results if requested.

 

All incoming material is visually inspected and PMI (Positive Material Identification) tested before processing begins and all our production material is checked during each stage of processing.

 

All incoming orders are produced to the individual customer specification, some of which may involve processing sample batches for testing prior to full production.

 

Final Inspection carried out on all finished material to include:

Visual inspection

Dimensional checks

PMI (Positive Material Identification)

Mechanical tests

 

Nickel Alloy Material Available Formats

Fushun offers pure Nickel alloy materials in a variety of forms, including:

Seamless & welded pipe

Seamless & welded tube

Bar

Wire

Sheet

Plate

Forgings

Pipe fittings

Flanges

Weld Rod

 

Nickel Alloy Supply Quantities for Single Items or Full Bills

At Fushun, we can supply single items or full bills of nickel alloy materials for most any project. No inquiry is too small. We offer quick responses to customer inquiries and specialize in the rapid delivery of both large and small quantities of nickel alloy products.

 

Contact Fushun for Nickel Alloy Materials Today

Contact us for more information regarding our nickel alloy material options, or request a quote for further pricing details today. Fushun is your trusted nickel alloy supplier and manufacturer of premium nickel alloy materials.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x