manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

Hot Rolled Mill Work Rolls

Hot Rolled Mill Work Rolls

Hot Rolled Mill Work Rolls

Introduce

Hot Strip Mill Work Rolls account for a substantial part of our global output. We provide high quality products from our facilities in Europe, North America, and Asia, when and where they are required, anywhere in the world.

 

An extensive range of roll dimensions and materials

Our plants can manufacture almost any size or grade of Hot Strip Mill Work Rolls for all applications ranging from Roughing Mill Work Rolls, including Vertical Edgers, to Finishing Stand Work Rolls.

 

Manufacturing

Forged rolls are manufactured at our plants in the China. We also provide customers with re-hardening and re-cutting service and support.

 

With FUSHUN extensive knowledge and experience of manufacturing forged work rolls, we can assist clients in selecting the grades and parameters that will assure optimal performance in their mill operations.

 

Process

Product design → Smelting (EF + ESR) → Forging → (Normalizing) → Spheroidizing and hydrogen annealing → Rough turning of the roll surface (cut test block) → Inspection (UT, macroscopic, microscopic, dimensions, appearance) → Storage and material requisition → Rough machining → Ultrasonic testing → Quenching and tempering treatment → Hardness inspection → Semi-finish machining → Roll neck surface and thrust end surface quenching and tempering → Roll neck hardness inspection → Semi-finish machining → Ultrasonic testing → Roll body surface quenching (+ cold treatment + low-temperature tempering) → Roll body hardness inspection → Finish machining → Inspection → Storage → Rust prevention and packaging → Transportation

 

Advantages

  • ESR steel ingots have high purity.
  • Heat treatment is good, and hardness is uniform.
  • Machining dimensions are precise.
  • No burn issues caused by grinding.

 

Main Roll Grades

The following list presents the different grades that FUSHUN can provide. Further information is available in our Product Data Sheets.

 

Steel Grade C Si Mn Cr Ni Mo V
55Cr 0.50-0.60 0.17-0.37 0.35-0.65 1.00-1.30 ≤0.30 / /
50CrMnMo 0.45-0.55 0.20-0.60 1.30-1.70 1.40-1.80 / 0.20-0.60 /
60CrMnMo 0.55-0.65 0.25-0.40 0.70-1.00 0.80-1.20 0.25 0.20-0.30 /
50CrNiMo 0.45-0.55 0.20-0.60 0.50-0.80 1.40-1.80 1.00-1.50 0.20-0.60 /
60CrNiMo 0.55-0.65 0.20-0.40 0.60-1.00 0.70-1.00 1.50-2.00 0.10-0.30 /
60SiMnMo 0.55-0.65 0.70-1.10 1.10-1.50 / / 0.30-0.40 /
60CrMoV 0.55-0.65 0.17-0.37 0.50-0.80 0.90-1.20 / 0.30-0.40 0.15-0.35
70Cr3NiMo 0.60-0.80 0.40-0.70 0.50-0.90 2.00-3.00 0.40-0.60 0.25-0.60 /

*P, S, ≤0.025 ; Cu≤0.25

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x