manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

F51 Duplex Stainless Steel

Duplex Steel F51 (UNS S31803) / F60 (UNS 32205) / 1.4462

SCM435 Alloy Steel

A duplex austenitic-ferritic chromium-nickel-molybdenum stainless steel.

F51 Duplex Stainless Steel combines improved resistance to stress corrosion cracking, pitting, crevice corrosion and high strength. Due to it’s chemical composition F51 duplex stainless steel resists chloride environments and sulphide stress corrosion.

 

<<DATA SHEET>>

 

Technical challenges

We can effectively control the temperature at the beginning and end of the forging process, as well as manage the temperature during solution treatment, ensuring it meets the requirements for low-temperature impact.

 

Chemical Composition Limits

Weight% C Mn P S Si Cr Ni Mo N
Duplex F51 0.03 max 2.0 max 0.03 max 0.02 max 1 max 21-23 4.5-6.5 2.5-3.5 0.80-0.20

 

EN 10088-3

Mechanical Property Value
Proof Stress 450 Min MPa
Tensile Strength 650 to 880 MPa
Elongation A50 mm 25 Min %
Hardness Brinell 270 Max HB

 

Physical Property Value
Density 7.805 g/cm³
Thermal Expansion 13.7 x10-6/K
Modulus of Elasticity 200 GPa
Thermal Conductivity 19.0 W/m.K
Electrical Resistivity 0.85 x10-6 Ω .m

 

Availability

Duplex F51 is available in Plate, Sheet, Round Bar, Flat Bar and Forging Stock for sizes contact Sales.

 

Specifications

ASTM A182 F51 / F60

ASTM A276 F51 / F60

ASTM A479 F51

AISI F51

BS 318S13 (Wrought)

BS 332C15 (Cast)

WS 1.4462

WS 1.4470

X2CrNiMoN22.5.3

AFNOR Z2CND22.05Az

UNS S31803

UNS S32205

SAF2205 – SANMAC (Brand name)

URANUS 45N (Brand name)

FALC223 (Brand name)

 

Characteristics

Higher strength than standard stainless steels

Higher corrosion resistance than Alloy 316L stainless steel in a wide variety of corrosive chemicals including sulphuric, phosphoric and nitric acids

Good resistance to pitting and crevice corrosion in seawater

High stress corrosion resistance

Lower thermal expansion than austenitic stainless steels

Higher thermal conductivity than austenitic stainless steels

 

Applications

  • Process industry components in sulphuric acid, nitric acid, phosphoric acid, ethylene oxide, polypropylene & PVC production
  • Equipment handling organic & fatty acids, chemical storage, tankers, heat exchangers
  • Marine industry and shipbuilding propellers, shafts, rudders, shaft seals, pumps, bolts, fasteners, valves, instrumentation
  • Oil and chemical tankers
  • Oil & Gas industry pumps, valves, pipe, vessels, wellhead equipment, subsea equipment, separators, heat exchangers
  • Pollution control systems, effluent scrubbing, flue gas desulphurisation (FGD)
  • Waste water treatment, sour water purification
  • Pulp & paper industry applications such as pulp liquor heaters, bleach tower linings, digesters, brownstock washers
  • Food industry applications including brewery piping, evaporators, hot liquor tanks, presses

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x