manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

Compression Mould Tool Steel

Compression Mould Tool Steel

Compression Mould Tool Steel

Fushun are main manufacturer of tool steel for Compression Mould.

 

What is Compression Mould?

A compression mold is a specialized manufacturing tool designed for the compression molding process, consisting of a matching top and bottom mold that works under heat and pressure. The mold typically includes a cavity in the lower portion and a force-applying plunger or plug in the upper portion. Unlike Compression molds, compression molds operate by directly compressing pre-placed material rather than injecting it, making them particularly suitable for larger parts and thermoset materials.

The main function of compression molds is to shape materials through the application of heat and pressure, transforming raw materials such as thermoset compounds, rubber, or composite materials into finished products. During the process, the mold not only shapes the material but also facilitates the chemical curing reaction in thermoset materials. These molds are designed with specific features including flash channels, air vents, heating elements, and ejection systems to ensure proper material flow, curing, and part removal.

Compression molds require materials with specific properties to withstand the unique challenges of the compression molding process. The mold materials must possess excellent heat resistance, high compressive strength, and good thermal conductivity. They also need to demonstrate superior wear resistance and dimensional stability at elevated temperatures. The mold surfaces often receive special treatments or coatings to prevent material adhesion and enhance release characteristics, while also improving the mold’s resistance to thermal fatigue and chemical reactions from the molding compounds.

 

Compression Mould Materials

1.2825 95MnWCr5 MnCrWV
1.2824 70MnMoCr8 7CrMn2Mo
H11 SKD6 1.2343 X37CrMoV5-1 4Cr5MoSiV
H13 SKD61 1.2344 X40CrMoV5-1 4Cr5MoSiV1
1.1191 C45U SM45
  SM50
    SM55
P20 1.2311 35CrMo7 3Cr2Mo

 

Chemical Composition of Compression Mould

Grade C Si Mn Cr W Mo V
MnCrWV 0.90~1.05 0.10~0.40 1.05~1.35 0.50~0.70 0.50~0.70   0.05~0.15
7CrMn2Mo 0.65~0.75 0.10~0.50 1.80~2.50 0.90~1.20   0.90~1.40  
4Cr5MoSiV 0.33~0.43 0.80~1.20 0.20~0.50 4.75~5.50 1.10~1.60 0.30~0.60
4Cr5MoSiV1 0.32~0.45 0.80~1.20 0.20~0.50 4.75~5.50   1.10~1.75 0.80~1.20
SM45 0.42~0.48 0.17~0.37 0.50~0.80        
SM50 0.47~0.53 0.17~0.37 0.50~0.80        
SM55 0.52~0.58 0.17~0.37 0.50~0.80      
3Cr2Mo 0.28~0..40 0.20~0.80 0.60~1.00 1.40~2.00   0.30~0.55  

 

Properties of Compression Mould Steel

Grade Annealed HBW
MnCrWV ≤255
7CrMn2Mo ≤235
4Cr5MoSiV ≤229
4Cr5MoSiV1 ≤229
SM45 155~215
SM50 165~225
SM55 170~230
3Cr2Mo 235

 

Available Shapes from Fushun

*Round Bar

*Flat Bar

*Block

*Plate

 

Contact Information

info@fushunspecialsteel.com

Welcome your inquiry. We will send you a free quotation within 24 hours.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x