Most Common Tool Steel Grades with Applications

Most Common Tool Steel Grades with Applications Tool steels are divided into 5 groups. Each of them has specific features regarding aspects like surface hardness, strength or toughness, working temperature, shock resistance and cost. These five groups of tool steel are: Water-hardening tool steel Cold-working tool steel

Read more

Effect of 18CrNiMo7-6 steel deep carburizing process on tissue properties

Effect of 18CrNiMo7-6 steel deep carburizing process on tissue properties   In the last decade or so, the high speed development of wind power generation, high speed railway, etc., European standard 18CrNiMo7-6 steel is widely used in the manufacture of wind power gearbox gears, large modulus gears,

Read more

Chinese SpecialSteel Factory S690 Forging Steel for largest wind turbine tower crane

On October 1, XCMG XGL1800 wind turbine tower crane, made of S690 forged round steel, was used to lift a 3.0 MW wind turbine to a height of over 140m in a soft geological environment with strong winds of up to grade 6 in the Yulin Dapu

Read more

Breakthroughs! Ttitanium alloy rod production line successful by MCC EPC

On August 18, 2020, the heat load test run of the titanium alloy small bar production line of Shaanxi Tiancheng Aviation Materials Co., Ltd., which was general contracted by MCC Jingcheng EPC, was successful, marking that MCC Jingcheng’s long products business successfully entered non-ferrous metals Rolling field.

Read more

Martensitic stainless steels

Martensitic stainless steels are characterized by high strength and hardness in the heat treated condition. We offer a range of martensitic stainless alloys which contain 11 – 17% chromium with 0.15 – 0.63% carbon. Martensitic grades are magnetic in both the annealed and hardened (heat treated) condition.

Read more

Ferritic stainless steels

Ferritic stainless steels are classified in the 400 series, usually with 10% to 30% chromium content, and are often chosen for their excellent corrosion resistance and elevated temperature oxidation resistance. With greater strength than carbon steels, ferritics provide an advantage in many applications where thinner materials and

Read more

Precipitation Hardening (PH) stainless steels

Precipitation Hardening (PH) stainless steels are classified as martensitic or semi-austenitic. They develop their high strength and hardness through a variety of heat treatments resulting in a very high strength-to-weight ratio. Semi-austenitic grades are 17-7 PH® and PH 15-7 Mo®. They are austenitic in the annealed state,

Read more

Introduce Duplex Stainless Steels

Duplex stainless steels contain a mixture of austenite and ferrite in their structure, and exhibit characteristics of both phases with higher strength and ductility. Nitrogen is added to the second generation duplex alloys and provides strength and improved weldability.Type 2205 duplex stainless steel is a grade that

Read more

What is the difference between 718H mold steel and P20H mold steel?

What are the characteristics of 718H mold steel? What are the characteristics of P20 die steel? What is the difference between 718 mold steel and P20H mold steel?   A: 718H mold steel, corresponding to Chinai’s 3Cr2NiMo mold steel. **Features** 718H is an improved steel grade of

Read more

Why is duplex stainless steel used in the cooling water system of nuclear power plants?

The World Nuclear Association’s annual report shows that the global nuclear power generation in 2018 exceeded 250 billion kWh, accounting for 10.5% of the global power supply. As of June 2019, 54 nuclear power plants are under construction worldwide. As a clean energy, nuclear power is a

Read more

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x