Improving Comprehensive Yield Rate of H13 Die Steel Forging: A Technical Analysis

Improving Comprehensive Yield Rate of H13 Die Steel Forging: A Technical Analysis In the field of hot work die steel manufacturing, FUSHUN METAL has conducted extensive research on improving the comprehensive yield rate of H13 die steel forgings. This analysis explores the key factors affecting yield rates

Read more

Chinese New Year Holiday Notice 2025

Dear Valued Customers, We would like to inform you that Fushun Metal will be closed for the Chinese New Year holiday from January 24th to February 5th, 2025. We will resume normal operations on February 6th, 2025. During this period, our email address info@fushunspecialsteel.com will remain monitored

Read more

Research on the Process to Improve the Uniformity of Eutectic Carbides in Tool Steel

Cr12MoV tool steel is a typical cold-work tool steel, accounting for 17% of the total tool steel production and 34% of alloy tool steel production. It has excellent hardenability, quenching and tempering hardness, wear resistance, and strength. It is used to manufacture various cold punching dies and

Read more

Tempering Microstructure and Hardness of P20 Plastic Mold Steel

Introduction P20 plastic mold steel is a widely utilized material due to its simple metallurgical production process, high yield rate, and affordability. It exhibits good machinability within the pre-hardened hardness range of 28–35 HRC, excellent hardenability for achieving uniform hardness in large cross-sections, and superior mirror polishing

Read more

Empowering Our Team for a Stronger Future – 2024 Strategic Training in Shenzhen

At Fushun Special Steel, we believe that our employees are the foundation of our success. As part of our commitment to growth and development, we are proud to announce a high-impact training program for our Finance, Sales, and Procurement Department Managers, scheduled to take place in mid-December

Read more

Ultrasonic Testing Based Method for Detecting Internal Defects in H13 Tool Steel

H13 tool steel, known for its excellent thermal stability, wear resistance, and high toughness, is widely used in hot working molds. However, during the casting and processing of mold steel, internal defects can occur, which become a critical factor limiting the performance and service life of mold

Read more

Effect of Aging Process on Low-Temperature Mechanical Properties of 15-5PH Steel

Effect of Aging Process on Low-Temperature Mechanical Properties of 15-5PH Steel 15-5PH steel is a widely used precipitation-hardened stainless steel in the aerospace field. When cooled from the solution temperature to room temperature, its microstructure transforms into quenched martensite. After aging, due to the precipitation of copper-rich

Read more

Improvement Measures for Transverse Charpy Impact Strength of Hot Work Tool Steel 1.2344

Improvement Measures for Transverse Charpy Impact Strength of Hot Work Tool Steel 1.2344 As a high-quality heat-resistant tool steel, 1.2344 is known for its uniform composition, good hardenability, excellent machinability, high toughness, hardness, low-temperature wear resistance, and high-temperature fatigue resistance. It is particularly widely used in die-casting

Read more

The control of cleanliness during the electroslag remelting (ESR) process of die steel 1.2083

The control of cleanliness during the electroslag remelting (ESR) process of die steel 1.2083 is as follows: Die steel is an important industrial material widely used in aerospace, automotive manufacturing, electronics, toys, medical devices, and many other fields. To improve the cleanliness, wear resistance, and impact resistance

Read more

The control of inclusions during the electroslag remelting (ESR) process of duplex stainless steel F55

The control of inclusions during the electroslag remelting (ESR) process of duplex stainless steel F55 is as follows: Duplex stainless steel F55 has high strength, good formability and weldability, excellent resistance to localized corrosion and stress corrosion cracking caused by chlorides. Typical applications include petrochemicals, fertilizer industries,

Read more

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x