In addition to providing the widest range of materials to many different sectors, we are the only company who can melt and forge according to customer requests and produce in the form closest to the final product. We provide services that will increase the added value in products by adding our mechanical processing and heat treatment capabilities to our forging products, which are produced in requested forms from automotive to energy, from maritime to mold industry.

 

Stainless Steel 422 (AMS 5655)

Alloy 422 is a hardenable stainless steel designed for use at temperatures of up to 1200ºF (649ºC). Alloy 422 has good resistance to scaling and oxidation. Through heat treatment, high mechanical properties can be developed. Alloy 422 is used in applications such as compressors or steam turbines and also in aircraft parts, valves, high temperature bolting etc.

 

Specifications

UNS S42200

AISI 616

AMS 5655 Bars / wire/ forging H&T

ASTM A 565 GRD 616

DOD F 24669/7

MIL S 861

B50A125 (Cap of)

B50A951A1 (Cap of)

BS 970; 442S19

EN61

 

Applications:

  • Aircraft parts
  • Steam and gas turbine components
  • High heat components
  • Rotors

 

Chemical Component

Grade UNS Carbon Manganese Phosphorus Sulfur Silicon Chromium Nickel Molybdenum Vanadium Tungsten
616 S42200 0.20–0.25 0.50–1.00 0.025 0.025 0.50max 11.00–12.50 0.50–1.00 0.90–1.25 0.20–0.30 0.90–1.25

 

Mechanical Properties

Material Condition 0.2 % Yield Strength (ksi) Ultimate Tensile Strength (ksi) % Elongation in 2″ % Reduction of Area Hardness HB
Alloy 422 Hardened & Tempered (AMS 5655) 140 115 13 25 293-341

 

Machineability

  • Comparable to 18-8 but easier to machine
  • Help avoid galling with sharply ground tools
  • Maintain consistent speed and feed
  • Turning tools: 8-14° side rake
  • Drilling: 140° point
  • Threading: grind tools with 10-15° back rake
  • Cobalt high-speed tools: turn at 90-120 sfpm, drill at 40-75 sfpm, mill at 70-120 sfpm, ream at 20-60 sfpm, roughing and finishing at 200-400 sfpm

 

Workability

  • Initial forging and rolling at 2100° to 2150°F (1149° to 1177°C)
  • 1700°F (927°C) minimum to hot work

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x