manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

AISI 444 1.4521 Stainless Steel

AISI 444 1.4521 Stainless Steel

AISI 444 is a low carbon, dual stabilised, molybdenum containing ferritic stainless steel with good ductility, toughness and resistance to sensitisation, even in the welds. With 18% chromium and 2% molybdenum, the steel has good pitting resistance and crevice corrosion resistance, similar to CS316 and good general corrosion resistance and oxidation resistance, similar to 316 in most environments. Being a ferritic stainless steel, AISI 444 is not susceptible to Stress Corrosion Cracking. Annealed AISI 444 is ductile and can be formed using a wide range of roll forming or mild stretch bending operations as well as the more common drawing and bending operations. AISI 444 does not harden excessively during cold working.

 

Characteristics

> Excellent resistance to chloride pitting and crevice corrosion cracking

> Immune to Chloride ion stress corrosion

> Maintains high strength at elevated temperatures

> Resistant to sea water, in both flowing and stagnant condition

>Heat resistant

 

Applications

> Marine engineering

> Furnaces a gas turbines

>Chemical processing plants

> Boiler a pressure vessels

> Nuclear power plants

 

Equivalent

Euronorm Nom. AISI / ASTM / UNS
1.4521 X2CrMoTi18-2 444

 

Chemical Composition

Type C Mn Si P S Cr Mo Ni Nb Ti
444 0.025 max 1.00 max 1.00 max 0.040 max 0.030 max 71.5-19.50 1.75-2.50 1 1 0.20+4(C+N) 0.80

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

5 +AT: Solution annealed

6 +P: Precipitation hardened

Suface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mechanical Properties

Type Product Form 0.2% Proof Stress (Mpa) Tenstile Strength (Mpa) Elongation (%) Brinell Hardness
444 C 275 min 415 min 20 min 217

 

Delivery Condition

Stress Relieved Annealed

Bright Annealed

Normalized

Solution Treatment

 

CORROSION RESISTANCE

Type 444 provides excellent corrosion resistance in moderately severe environments of many types that include chlorides and organic acids found in foods and beverages. It also provides satisfactory resistance to dilute sulfuric acid solutions and to highly concentrated sodium hydroxide.

 

FORMABILITY

Type 444 provides excellent formability and can be readily deep drawn and spin formed. Stretch forming, however, is limited in application for this material.

 

WELDABILITY

The ferritic class of stainless steels is generally considered to be weldable by the common fusion and resistance techniques.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x