manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

Precision Stamping Mould Tool Steel

Precision Stamping Mould Tool Steel

Precision Stamping Mould Tool Steel

Fushun are main manufacturer of tool steel for Precision Stamping Mould.

 

What is Precision Stamping Mould?

Precision stamping Moulds are highly sophisticated tooling systems designed for manufacturing parts with extremely tight tolerances and superior surface finish. These Moulds are built with exceptional precision, incorporating precise alignment systems, advanced guiding mechanisms, and carefully engineered clearances. Unlike conventional stamping Moulds, precision Moulds often feature additional refinements such as compound operations and progressive staging to achieve higher accuracy.

 

The main function of precision stamping Moulds is to produce components that require exceptional dimensional accuracy, typically with tolerances as tight as ±0.01mm. They are extensively used in industries such as electronics, medical devices, aerospace, and precision instruments where component accuracy is crucial. These Moulds can perform multiple operations including blanking, piercing, forming, and coining while maintaining consistent quality and repeatability throughout high-volume production runs.

 

The materials used in precision stamping Moulds require specific compositions to achieve optimal performance. Premium grade tool steels such as M4 or ASP series contain high amounts of tungsten (up to 6%), molybdenum (5%), chromium (4%), and vanadium (4%) to provide superior wear resistance and dimensional stability. These materials achieve extreme hardness levels (62-65 HRC) while maintaining adequate toughness. Special surface treatments like PVD (Physical Vapor Deposition) coatings are often applied to enhance wear resistance and reduce friction. The matrix material’s fine carbide distribution and uniform microstructure are essential for maintaining sharp cutting edges and preventing premature wear under high-precision stamping conditions.

Precision Stamping Mould Materials

O2 1.2842 9Mn2V
  70MnMoCr8 7CrMn2Mo
  6Cr4W3Mo2VNb
    6W6Mo5Cr4V
  W6Mo5Cr4V2
  7Cr7Mo2V2Si
A2 SKD12 1.2363 X100CrMoV5 Cr5Mo1V
D2 SKD10 1.2379 X153CrMoV12 Cr12Mo1V1
L6 SKT4 1.2714 55NiCrMoV7 5CrNi2MoV
    4Cr5W2VSi
H21 SKD5 1.2581 X30WCrV9-3 3Cr2W8V
H11 SKD6 1.2343 X37CrMoV5-1 4Cr5MoSiV
H13 SKD61 1.2344 X40CrMoV5-1 4Cr5MoSiV1
H10 1.2365 4Cr3Mo3SiV
  5Cr4Mo3SiMnVA1
H12 1.2605 X35CrWMoV5 4Cr5MoWVSi
  3Cr3Mo3W2V
      4Cr5Mo2V
SKD7   32CrMoV12-28 3Cr3Mo3V

 

Chemical Composition of Precision Stamping Mould

Grade C Si Mn Cr W Mo Ni V Co
9Mn2V 0.85~0.95 ≤0.40 1.70~2.00         0.10~0.25  
7CrMn2Mo 0.65~0.75 0.10~0.50 1.80~2.50 0.90~1.20   0.90~1.40      
6Cr4W3Mo2VNb 0.60~0.70 ≤0.40 ≤0.40 3.80~4.40 2.50~3.50 1.80~2.50   0.80~1.20  
6W6Mo5Cr4V 0.55~0.65 ≤0.40 ≤0.50 3.70~4.30 6.00~7.00 4.50~5.50   0.70~1.10  
W6Mo5Cr4V2 0.80~0.90 0.15~0.40 0.20~0.45 3.80~4.40 5.50~6.75 4.50~5.50   1.75~2.20  
7Cr7Mo2V2Si 0.68~0.78 0.70~1.20 ≤0.40 6.50~7.50   1.90~2.30   1.80~2.20
Cr5Mo1V 0.95~1.05 ≤0.50 ≤1.00 4.75~5.50   0.90~1.40   0.15~0.50  
Cr12Mo1V1 1.40~1.60 ≤0.60 ≤0.50 11.00~13.00   0.70~1.20   0.50~1.10 ≤1.00
5CrNi2MoV 0.50~0.60 0.10~0.40 0.60~0.90 0.80~1.20   0.35~0.55 1.50~1.80 0.05~0.15  
4Cr5W2VSi 0.32~0.42 0.80~1.20 ≤0.40 4.50~5.50 1.60~2.40     0.60~1.00  
3Cr2W8V 0.30~0.40 ≤0.40 ≤0.40 2.20~2.70 7.50~9.00     0.20~0.50  
4Cr5MoSiV 0.33~0.43 0.80~1.20 0.20~0.50 4.75~5.50 1.10~1.60    0.30~0.60  
4Cr5MoSiV1 0.32~0.45 0.80~1.20 0.20~0.50 4.75~5.50   1.10~1.75   0.80~1.20   
4Cr3Mo3SiV 0.35~0.45 0.80~1.20 0.25~0.70 3.00~3.75   2.00~3.00   0.25~0.75  
5Cr4Mo3SiMnVA1 0.47~0.57 0.80~1.10 0.80~1.10 3.80~4.30   2.80~3.40   0.80~1.20   
4Cr5MoWVSi 0.32~0.40 0..80~1.20 0.20~0.50 4.75~5.50 1.10~1.60 1.25~1.60    0.20~0.50  
3Cr3Mo3W2V 0.32~0.42 0.60~0.90 ≤0.65 2.80~3.30 1.20~1.80 2.50~3.00   0.80~1.20   
4Cr5Mo2V 0.35~0.42 0.25~0.50 0.40~0.60 5.00~5.50   2.30~2.60   0.60~0.80  
3Cr3Mo3V 0.28~0.35 0.10~0.40 0.15~0.45 2.70~3.20   2.50~3.00   0.40~0.70  
4Cr5Mo3V 0.35~0.40 0.30~0.50 0.30~0.50 4.80~5.20    2.70~3.20 0.40~0.60  
3Cr3Mo3VCo3 0.28~0.35 0.10~0.40 0.15~0.45 2.70~3.20   2.60~3.00   0.40~0.70 2.50~3.00

 

Properties of Precision Stamping Mould Steel

 

Grade Annealed HBW Hardened HRC min.
9Mn2V ≤229 62
7CrMn2Mo ≤235 61
6Cr4W3Mo2VNb ≤255 60
6W6Mo5Cr4V ≤269 60
W6Mo5Cr4V2 ≤255 63
7Cr7Mo2V2Si ≤255 60
Cr5Mo1V ≤255 60
Cr12Mo1V1 ≤255 59
5CrNi2MoV ≤255  
4Cr5W2VSi ≤229  
3Cr2W8V ≤255  
4Cr5MoSiV ≤229  
4Cr5MoSiV1 ≤229  
4Cr3Mo3SiV ≤229  
5Cr4Mo3SiMnVA1 ≤255  
4Cr5MoWVSi ≤235  
3Cr3Mo3W2V ≤255  
4Cr5Mo2V ≤220  
3Cr3Mo3V ≤229  
4Cr5Mo3V ≤229  
3Cr3Mo3VCo3 ≤229  
5CrNiMnMoVSCa ≤255  
00Ni18Co8Mo5TiAl ≤229  

 

Available Shapes from Fushun

*Round Bar

*Flat Bar

*Block

*Plate

 

Contact Information

info@fushunspecialsteel.com

Welcome your inquiry. We will send you a free quotation within 24 hours.

 

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x