Fushun are main manufacturer of tool steel for Blanking Mould.

 

What is Blanking Mould?

A blanking Mould is a specialized tool used in the manufacturing and metalworking industry to perform the process of blanking, which is a type of shearing operation. In this process, a punch and Mould are utilized to cut out a piece of material from a larger sheet or strip, producing a component known as a blank. The blank is typically a flat piece that will undergo further processing or assembly to become a finished part.

 

Components of a Blanking Mould:

  1. Punch (Male Component): This part descends and applies force to the material, pushing it through the Mould.
  2. Mould(Female Component): A cavity or opening shaped to the desired outline of the blank. The material is sheared along the edges of this cavity.

 

How the Blanking Process Works:

– A sheet of material (commonly metal) is placed between the punch and Mould.

– The punch presses down with enough force to shear the material along the contour of the Mould opening.

– The sheared piece (the blank) separates from the surrounding material.

– The blank falls through the Mould or is ejected for further processing.

– The remaining material, often called scrap or skeleton, may be recycled or discarded.

 

A blanking Mould is an essential tool in modern manufacturing, enabling the efficient and precise cutting of material blanks from larger sheets. By leveraging the mechanical force of a punch and Mould setup, manufacturers can produce high-quality components rapidly and cost-effectively. This process is foundational in industries that demand consistent, accurate parts for the assembly of complex products.

Blanking Mould Materials

O2 1.2842 9Mn2V
O1 SKS3 1.2510 95MnCr5 9CrWMn
SKS31   CrWMn
1.2825 95MnWCr5 MnCrWV
1.2824 70MnMoCr8 7CrMn2Mo
  Cr8Mo2SiV
  Cr4W2MoV
  6Cr4W3Mo2VNb
D3 SKD1 1.2080 X210Cr12 Cr12
SKD2   X210CrW12 Cr12W
  7Cr7Mo2V2Si
A2 SKD12 1.2363 X100CrMoV5 Cr5Mo1V
D2 SKD10 1.2379 X153CrMoV12 Cr12Mo1V1
  8Cr3
H10 1.2365 4Cr3Mo3SiV
A8 1.2360 X48CrMoV8-1-1 5Cr5WMnSi

 

Chemical Composition of Blanking Mould

Grade C Si Mn Cr W Mo V Nb Co
9Mn2V 0.85~0.95 ≤0.40 1.70~2.00       0.10~0.25    
9CrWMn 0.85~0.95 ≤0.40 0.90~1.20 0.50~0.80 0.50~0.80      
CrWMn 0.90~1.05 ≤0.40 0.80~1.10 0.90~1.20 1.20~1.60        
MnCrWV 0.90~1.05 0.10~0.40 1.05~1.35 0.50~0.70 0.50~0.70   0.05~0.15    
7CrMn2Mo 0.65~0.75 0.10~0.50 1.80~2.50 0.90~1.20   0.90~1.40      
Cr8Mo2SiV C.95~1.03 0.80~1.20 0.20~0.50 7.80~8.30   2.00~2.80 0.25~0.40    
Cr4W2MoV 1.12~1.25 0.40~0.70 ≤0.40 3.50~4.00 1.90~2.60 0.80~1.20 0.80~1.10    
6Cr4W3Mo2VNb 0.60~0.70 ≤0.40 ≤0.40 3.80~4.40 2.50~3.50 1.80~2.50 0.80~1.20 0.20~0.35  
Cr12 2.00~2.30 ≤0.40 ≤0.40 1.50~13.00          
Cr12W 2.00~2.30 0.10~0.40 0.30~0.60 11.00~13.00 0.60~0.80        
7Cr7Mo2V2Si 0.68~0.78 0.70~1.20 ≤0.40 6.50~7.50   1.90~2.30 1.80~2.20  
Cr5Mo1V 0.95~1.05 ≤0.50 ≤1.00 4.75~5.50   0.90~1.40 0.15~0.50    
Cr12Mo1V1 1.40~1.60 ≤0.60 ≤0.50 11.00~13.00   0.70~1.20 0.50~1.10   ≤1.00
8Cr3 0.75~0.85 ≤0.40 ≤0.40 3.20~3.80           
4Cr3Mo3SiV 0.35~0.45 0.80~1.20 0.25~0.70 3.00~3.75   2.00~3.00   0.25~0.75  
5Cr5WMnSi 0.50~0.60 0.75~1.10 0.20~0.50 4.75~5.50 1.00~1.50 1.15~1.65      

 

Properties of Blanking Mould Steel

Grade Annealed HBW Hardened HRC min.
9Mn2V ≤229 62
9CrWMn 197~241 62
CrWMn 207~255 62
MnCrWV ≤255 62
7CrMn2Mo ≤235 61
Cr8Mo2SiV ≤255 62
Cr4W2MoV ≤269 60
6Cr4W3Mo2VNb ≤255 60
Cr12 217~269 60
Cr12W ≤255 60
7Cr7Mo2V2Si ≤255 60
Cr5Mo1V ≤255 60
Cr12Mo1V1 ≤255 59
8Cr3 207~255  
4Cr3Mo3SiV ≤229  
5Cr5WMnSi ≤248  

 

Available Shapes from Fushun

*Round Bar

*Flat Bar

*Block

*Plate

 

Contact Information

info@fushunspecialsteel.com

Welcome your inquiry. We will send you a free quotation within 24 hours.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x