manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

1.4876, N08800, Alloy 800, Heat Resisting Austenitic Steel

1.4876, N08800, Alloy 800, Heat Resisting Austenitic Steel

 

1.4835 X9CrNiSiNCe21-11-2 Austenitic Heat Resisting Stainless Steel

1.4876, also known as N08800 or Alloy 800, is a high-nickel alloy with excellent resistance to high-temperature corrosion and oxidation. It falls into the category of austenitic stainless steels and is specifically designed to perform well in elevated temperature and aggressive environments. Alloy 800 is often used in applications that require resistance to carburization, nitriding, and other forms of high-temperature corrosion.

 

One of its notable applications is in the petrochemical industry, particularly in furnace components and heat-treating equipment. It is also employed in power generation and various high-temperature processing industries. Alloy 800’s remarkable high-temperature strength, creep resistance, and corrosion resistance, particularly in sulfur-containing atmospheres, make it a reliable choice for applications where thermal stability and corrosion resistance are paramount.

 

Our Supply

Smelting line: VIM,VAR, IM, ESR, PESR, LF, VD, AOD

Danieli roll line: round & flat diameter 150mm max

Forged line: 800mm max

Heat-treatment line: annealed, quenched tempered, solution

Machining line: Turning, Milling, CNC

Chemical Composition

BS EN AISI/ASTM C Si Mn max P max S max Cr Ni
1.4876 N08800/Alloy 800 max 0.12 max 1.0 max 2.0 0.030 0.015 19-23 30-34

 

* Al 0.15-0.60 Ti 0.15-0.60

Mechanical Properties

BS EN AISI/ASTM Heat condition Hardness HB max Proof strength Rp1.0 N/mm2 min. Tensile strength Elongation A% min. long products
1.4876 N08800/Alloy 800 +AT solution annealed 192 210 450-680 30

 

 

Our advantage of heat resisting steel

  • High creep limit and lasting strength;
  • Easy smelting and processing and good casting, forging and welding properties;
  • high oxidation resistance and corrosion resistance;
  • high high-temperature mechanical properties;
  • Small expansion coefficient and good thermal conductivity;
  • Good processability and economy.
  • Organization stability at high temperature
  • Low cost

What is heat resisting steel?

Heat resisting steel is a kind of special steel that can maintain good mechanical properties and antioxidant properties under high temperature environment. It has high temperature stability, oxidation resistance and creep resistance, can maintain high strength and hardness at high temperatures, not easy to soften and deformation.

 

Why choose heat resisting steel?

1. High-temperature stability:

heat resisting steel at high temperatures to maintain high strength and hardness, will not occur obvious softening and deformation.

 

2. Antioxidant properties:

heat resisting steel surface to form a dense layer of oxide film, can effectively prevent oxidation reaction, slow down the oxidation rate of the material.

 

3. Creep resistance:

heat resisting steel at high temperatures can resist plastic deformation and creep phenomenon, to maintain good shape stability and dimensional accuracy.

 

4. Good processing performance:

heat resisting steel has good plasticity and weldability, can be convenient for hot processing and welding.

 

 

Application of heat resisting steel

heat resisting steel is widely used in aerospace, energy, chemical industry and other fields, mainly including the following aspects:

1. Aerospace field:

heat resisting steel used in the manufacture of aero-engine turbine blades, turbine discs, combustion chambers and other components, as well as aerospace spacecraft insulation materials.

 

2. Energy field:

heat resisting steel used in the manufacture of thermal power plant boiler supercritical and ultra-supercritical boiler piping and heating surface, and nuclear power plant nuclear reactor pressure vessel and fuel components.

 

3. Chemical industry:

heat resisting steel is used in the manufacture of chemical equipment reactor, separator, oil cracker pipeline, etc., which can withstand high temperature, high pressure and corrosive media.

 

4. Other fields:

heat resisting steel is also widely used in metallurgy, machinery, automobile and other fields, used in the manufacture of a variety of parts and tools under high-temperature working environment.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x