manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

SCM415 Alloy Steel

SCM415 Alloy Steel

SCM415 whose surface are processed through carburizing hardening treatment are used for the parts which need high toughness or wear resistance, such as cylinder piston, crankshaft, gears, pin, shafts and so on.

 

SCM415 Steel is a high quality Quenched and Tempered Alloy Structural steel, It belong to the high quality medium carbon, Oil Quenched & Tempered Hardenss is 28-34 HRc.SCM415 Annealing delivery hardenss less than 250HB.

 

Our supply size :

Diameter : 80 to 600 mm ;

Length : 1000 to 9000 mm ;

 

Our advantage :

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

International Comparison of Materials

INTER  ISO JAPAN GERMANY CHINA
JIS DIN GB
15CrMo4 SCM415 15CrMo5 15CrMo

 

Chemical Composition(JIS G4051)

C(%) Si(%) Mn(%) P(%) S(%) Ni(%) Cr(%) Mo(%) Cu(%)
0.13-0.18 0.15-0.35 0.6-0.85 0≦0.03 0≦0.03 0≦0.25 0.9-1.2 0.15-0.30 0≦0.3

 

Applications

SCM415 steel is a alloy structural steel. It is used for engineering structural, like high tensile shafts, bolts and nuts, gears, pinions and spindles. Locomotive traction with the big gear, supercharger drive gear, pressure vessel, rear axle, gear load of connecting rod and a spring clip,SCM415 can also be used to under 2000 m deep well of oil drill pipe joint and the fishing Alloy, and can be used for bending machine mould, etc

 

Product Features:

  1. High strength in room temperature and elevated temperature.
  2. High notch tolerance.
  3. Simplified design for bolting configuration

 

Conditions of heat treatment

Annealing: 850℃ Furnace Cooling

Normalization: 850~900℃ Air Cooling

Hardening: 850~900℃ 1st Oil Cooling, 800~850℃ 2rd Oil Cooling

Tempering: 150~200℃ Air Cooling

 

Criterion for heat treating conditions revise:

Ac: 770~835℃

Ar: 770~700℃

Ms: 410℃

 

Mechanical properties

Tensile strength (kgf/mm²): ≧85

Elongation (%): ≧16

Cross section reduction rate (%): ≧40

Impact value (J/cm2): ≧7

Hardness (Hb) : 235~321

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mill test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

 

We also supply :

4130 , 4130 p+x , 4140 , 4330v mod , 4340 , 4145h mod , 4317

1.8509 , 1.6523 , 1.7707 , 1.6657 , 1.6587 , 1.6582 , 1.6773

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x