manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

1.2767 Annealed Machined FORGINGS FLAT BAR for middle east clients

1.2767 45NiCrMo16 Cold Work Tool Steel Annealed Machined FORGINGS FLAT BAR for middle east clients

1.2767 STEEL

 

1.2767 45NiCrMo16 is a higher carbon version of the standard 4¼% nickel air/oil hardening steel. 1.2767 achieves a good hardness and is suitable for applications demanding extra wear resistance.

 

Material properties: Due to the high nickel and corresponding carbon content, this material is a very evenly hardening, dimensionally stable steel with high toughness and resistance to impact and compressive stress.

 

1.2767 is Nickel cold work tool steel. Good hardenability and thougness. Ability for polishing, photoetching and erosion treatment. Application include forging tools, dies of all sort, shapes and sizes, hot forging and pressing tools for steel and metal. Moulds, bushings, piercers, etc.

1.2767

Application
Mould plates and inserts for the processing of thermo- plastics and thermosets, especially for high gloss polishes, e.g. for transparent melts and components with high surface requirements, mould components with high compressive and flexural stresses, embossing tools and other uses for which the above requirements are needed.

S.R.No Steel Grade Thickness/

Diameter

Width Length QTY Delivery Condition Surface Condition
               
    mm mm mm TONS    
1 1.2767 30 2000-2300 3500-5800 2.9 Annealed Black
2 1.2767 40 2000-2300 3500-5800 3.66 Annealed Black
3 1.2767 50 2000-2300 3500-5800 3.635 Annealed Black
4 1.2767 60 2000-2300 3500-5800 5.405 Annealed Black
5 1.2767 70 2000-2300 3500-5800 5.415 Annealed Black
6 1.2767 30 80 3000-5800 1.025 Annealed Machined
7 1.2767 30 100 3000-5800 0.96 Annealed Machined
8 1.2767 30 120 3000-5800 0.965 Annealed Machined
9 1.2767 30 150 3000-5800 0.93 Annealed Machined
10 1.2767 30 160 3000-5800 1.03 Annealed Machined
11 1.2767 30 180 3000-5800 1.105 Annealed Machined
12 1.2767 30 200 3000-5800 1.065 Annealed Machined
13 1.2767 30 220 3000-5800 1.11 Annealed Machined
14 1.2767 30 310 3000-5800 1.025 Annealed Machined
15 1.2767 50 120 3000-5800 1.276 Annealed Machined
16 1.2767 50 150 3000-5800 1.977 Annealed Machined
17 1.2767 50 160 3000-5800 2.055 Annealed Machined
18 1.2767 50 180 3000-5800 1.822 Annealed Machined
19 1.2767 50 200 3000-5800 1.04 Annealed Machined
20 1.2767 50 220 3000-5800 1.215 Annealed Machined
21 1.2767 50 250 3000-5800 0.835 Annealed Machined
22 1.2767 50 360 3000-5800 0.905 Annealed Machined
23 1.2767 60 150 3000-5800 2 Annealed Machined
24 1.2767 60 160 3000-5800 0.345 Annealed Machined
25 1.2767 60 180 3000-5800 2 Annealed Machined
26 1.2767 60 200 3000-5800 2 Annealed Machined
27 1.2767 80 300 3000-5800 2.495 Annealed Machined
28 1.2767 80 400 3000-5800 3.75 Annealed Machined
29 1.2767 100 220 3000-5800 1.57 Annealed Machined
30 1.2767 100 260 3000-5800 1.85 Annealed Machined
31 1.2767 100 360 3000-5800 2.55 Annealed Machined
32 1.2767 100 460 3000-5800 1.755 Annealed Machined
33 1.2767 120 460 3000-5800 1.795 Annealed Machined

 

We also supply :

1.2510/H10, 1.2842, 1.2379/D2, 1.2080/X210Cr12/D3, 1.2436, 1.2365, 1.2885, 1.2343, 1.2344/H13/SKD61, 1.2581/H21, 1.2709, 1.2345, 1.2738/P20NI, 1.2083/420J2, 1.2316, 1.2312/P20S, 1.23111.2764

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.