manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

AISI 321 1.4541 SUS321 S32100 Stainless Steel

AISI 321 Stainless Steel

aisi 321

aisi 321

Overview

Grade 321 stainless steel (1.4541) is a heat resistant grade supplied into numerous industry sectors. The key property of this grade is the added titanium content (5 x C%) stabilising the material and making its resistance to carbide precipitation when exposed to high temperatures and resistance to oxidation its main characteristics. Whilst retaining good strength and corrosion resistance when exposed to high temperatures, this grade of stainless steel like most austenitic grades will also maintain its strength and toughness at sub-zero temperatures, making this an excellent choice for various applications ranging from oil refinery equipment to automotive exhaust systems. This heat resistant grade of stainless steel has a maximum dry air service temperature of 850ºC.

 

Form of Supply

* Sheet * Plate * Round Bar * Wire * Tube & Pipe

 

Grade 321 is the grade of choice for applications in the temperature range of up to about 900 °C, combining high strength, resistance to scaling and phase stability with resistance to subsequent aqueous corrosion.

 

Grade 321H is a modification of 321 with higher carbon content, to provide improved high-temperature strength.

 

A limitation with 321 is that titanium does not transfer well across a high-temperature arc, so it is not recommended as a welding consumable. In this case grade 347 is preferred – the niobium performs the same carbide stabilization task but can be transferred across a welding arc. Grade 347 is, therefore, the standard consumable for welding 321. Grade 347 is only occasionally used as parent plate material.

 

Like other austenitic grades, 321 and 347 have excellent forming and welding characteristics, are readily brake or roll-formed and have outstanding welding characteristics. Post-weld annealing is not required. They also have excellent toughness, even down to cryogenic temperatures. Grade 321 does not polish well, so is not recommended for decorative applications.

 

Grade 304L is more readily available in most product forms, and so is generally used in preference to 321 if the requirement is simply for resistance to intergranular corrosion after welding. However, 304L has lower hot strength than 321 and so is not the best choice if the requirement is resistance to an operating environment over about 500 °C.

 

321 is a titanium stabilised chromium-nickel austenitic stainless steel with good strength and excellent corrosion resistance, as supplied in the annealed condition with a typical brinell hardness of 175.Characterised by high corrosion resistance in general atmospheric corrosive environments it exhibits excellent resistance to most oxidizing agents, general foodstuffs, sterilizing solutions, dyestuffs, most organic chemicals plus a wide variety of inorganic chemicals, also hot petroleum gases, steam combustion gases, nitric acid, and to a lesser extent sulphuric acid. It displays good oxidation resistance at elevated temperatures has excellent resistance to intergranular corrosion and has excellent weldability. 321 cannot be hardened by thermal treatment, but strength and hardness can be increased substantially by cold working, with subsequent reduction in ductility.

 

Used extensively for applications where the addition of titanium and its stabilizing effect as a carbide forming element allows it to be welded and/or used within the carbide precipitation range 430oC – 870oC without the risk of intergranular corrosion. These include Food Processing, Dairy Equipment, Chemical, Petrochemical, Transport and associated industries etc.

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

5 +AT: Solution annealed

6 +P: Precipitation hardened

Suface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Key Properties

These properties are specified for the flat-rolled products (plate, sheet, and coil) in ASTM A240/A240M. Similar but not necessarily identical properties are specified for other products such as pipe and bar in their respective specifications.

 

Composition

Typical compositional ranges for grade 321 stainless sheets of steel are given in table 1.

Table 1. Composition ranges for 321-grade stainless steel

Grade C Mn Si P S Cr Mo Ni N Other
321 min.
max

0.08
2.00 0.75 0.045 0.030 17.0
19.0
9.0
12.0
0.10 Ti=5(C+N)
0.70
321H min.
max
0.04
0.10
2.00 0.75 0.045 0.030 17.0
19.0
9.0
12.0
Ti=4(C+N)
0.70
347 min.
max
0.08 2.00 0.75 0.045 0.030 17.0
19.0
9.0
13.0
Nb=10(C+N)
1.0

 

Mechanical Properties

Typical mechanical properties for grade 321 stainless sheets of steel are given in table 2.

Table 2. Mechanical properties of 321-grade stainless steel

Grade Tensile Strength (MPa) min Yield Strength 0.2% Proof (MPa) min Elongation (% in 50 mm) min Hardness
Rockwell B (HR B) max Brinell (HB) max
321 515 205 40 95 217
321H 515 205 40 95 217
347 515 205 40 92 201

 

Physical Properties

Typical physical properties for annealed grade 321 stainless sheets of steel are given in table 3.

Table 3. Physical properties of 321-grade stainless steel in the annealed condition

Grade Density (kg/m3) Elastic Modulus (GPa) Mean Coefficient of Thermal Expansion (μm/m/°C) Thermal Conductivity (W/m.K) Specific Heat 0-100 °C (J/kg.K) Electrical Resistivity (nΩ.m)
0-100 °C 0-315 °C 0-538 °C at 100 °C at 500 °C
321 8027 193 16.6 17.2 18.6 16.1 22.2 500 720

 

Grade Specification Comparison

Approximate grade comparisons for 321 stainless sheets of steel are given in table 4.

Table 4. Grade specifications for 321-grade stainless steel

Grade UNS No Old British Euronorm Swedish SS Japanese JIS
BS En No Name
321 S32100 321S31 58B, 58C 1.4541 X6CrNiTi18-10 2337 SUS 321
321H S32109 321S51 1.4878 X10CrNiTi18-10 SUS 321H
347 S34700 347S31 58G 1.4550 X6CrNiNb18-10 2338 SUS 347

 

Possible Alternative Grades

Possible alternative grades to grade 321 stainless sheets of steel are given in table 5.

Table 5. Possible alternative grades to 321-grade stainless steel

Grade Why it might be chosen instead of 321
304L The requirement is for resistance to intergranular corrosion, not for high-temperature strength
3CR12 Only a mild “high temperature” environment is present… up to about 600 °C.
304H Only a mild “high temperature” environment is present… up to about 800 °C.
310 The temperature of the operating environment is up to about 1100 °C – too high for 321 or 321H.
S30815
(253MA)
The temperature of the operating environment is up to about 1150 °C- too high for 321 or 321H.

 

Corrosion Resistance

Equivalent to Grade 304 in the annealed condition, and superior if a weldment in these grades has not been post-weld annealed or if the application involves service in the 425-900 °C range. Subject to pitting and crevice corrosion in warm chloride environments, and to stress corrosion cracking above about 60 °C. Considered resistant to potable water with up to about 200 mg/L chlorides at ambient temperatures, reducing to about 150 mg/L at 60 °C.

 

Heat Resistance

Good oxidation resistance in intermittent service to 900 °C and in continuous service to 925 °C. These grades perform well in the 425-900 °C range, and particularly where subsequent aqueous corrosive conditions are present. 321H has higher hot strength and is particularly suitable for high-temperature structural applications.

 

Heat Treatment

Solution Treatment (Annealing) – heat to 950-1120 °C and cool rapidly for maximum corrosion resistance.

Stabilizing – heat to 870-900 °C for 1 hour per 25mm of thickness and air cool. Stabilization is recommended for most severe service conditions (above 425 °C) and particularly for material annealed at the upper side of the annealing temperature range.

Stress Relief – Heat to 700 °C for 1 to 2 hours and air cool.

These grades cannot be hardened by thermal treatment.

 

Welding

Excellent weldability by all standard fusion methods, both with and without filler metals. AS 1554.6 pre-qualifies welding of 321 and 347 with Grade 347 rods or electrodes; a high silicon version of 347 is also pre-qualified for welding of 321.

 

Applications

Typical applications include:

Aircraft exhaust manifolds

Expansion joints

Bellows

Furnace parts

Heating element tubing

Heat Exchangers

Woven or welded screens for high-temperature mineral processing

Spiral Welded tube for burner pipes and flues

 

Properties (MPa) Temperatures
600℃ 700℃ 800℃
Creep limit R1/1000 110 45 15
R1/10000 85 30 10
Creep resistance Rz/1000 200 88 30
Rz/10000 142 48 15
Rz/100000 65 22 10
Temperature T
°C/F
(°C/F)
Specific heat
J / kgK
(Btu / lb °F)
Thermal conductivity
W/mK
(Btu·in / ft2·h·°F)
Electric resistance
µΩ · cm
(Ω circ mill / ft)
Modulus of elasticity
kN/mm2
(103 ksi)
Expansion rate from 70°F bis T
10-6 / K
(10-6 / °F)
20 / 68 500 (-) 15 (-) 0,73 (-) 200 (-) 16,0 (-)
200 /392 186 (-) 16,5 (-)
300 / 572 179 (-) 17,0 (-)
400 / 752 172 (-) 17,5 (-)
500 / 932 165 (-) 18,0 (-)

 

temperature 0,2%Yield strength
in high temperatures
1,0% Yield strength
in high temperatures
°C / °F Rp 0,2 Rp 1,0
N/mm2 /ksi N/mm2 /ksi
100 / 212 176 / 25,50 208 / 30,16
200 / 392 157 / 22,77 186 / 30,00
300 / 572 136 / 19,70 167 / 24,20
400 / 752 125 / 18,10 156 / 22,60
500 / 932 119 / 17,00 149 / 21,60
ksi value calculated

Mechanical properties (20°C / 68°F)

1% Yield strength Rp1,0 (Mpa / ksi) 240 / 34,8
Tensile strength Rm (Mpa/ksi) 500-700
Elongation A5 (%) 40
impact work ISO-V 60 J

Temparature information

Application area
Operation temperature  ºF  to 1652 ºF
Explanation report air

 

Solution heat treatment
Working temperature 1886 ºF  to 2030 ºF
Processing informations cool down: water;air

 

Annealing
Working temperature 1832 ºF  to 2012 ºF
Explanation report duration 5 min; width 5 mm
Processing informations cool down: water;air

 

Solution heat treatment
Working temperature 2102 ºF  to 1562 ºF
Processing informations cool down: air

 

Standards / information

Standards Desciption
ASTM A 182 Standard Specification for Forged or Rolled Alloy-Steel Pipe Flanges,Forged Fittings and Valves and Parts for High-Temperature Service
ASTM A 213 Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler,Superheater,and Heat-Exchanger Tubes
ASTM A 240 sheet metal and ribbons from stainless Cr and Ni pressure containers
ASTM A 249 Standard Specification for Welded austenitic steel boiler, Superheaters, heat-exchangers,and condenser Tubes

 

alloy 321 is a general purpose austenitic stainless steel with a face centered cubic structure. It is essentially non-magnetic in the annealed condition and can only be hardened by cold working. Titanium is added to supress grain boundary Chromium Carbide precipitation and reduce susceptibilty to intergranular corrosion.

 

AISI 321 square bars hotrolled and pickled tolerance DIN EN 10059 ( formerly DIN 1014 ) long 4-6 mtr

Sizes:

25,00 mm 45,00 mm 65,00 mm 85,00 mm 135,00 mm
30,00 mm 50,00 mm 70,00 mm 90,00 mm 150,00 mm
35,00 mm 55,00 mm 75,00 mm 100,00 mm
40,00 mm 60,00 mm 80,00 mm 120,00 mm

1.4541 – AISI 321 hexagon bars hotrolled and pickled tolerance DIN EN 10059 ( formerly DIN 1014 ) long 4-6 mtr
Sizes:

41,00 mm 85,00 mm 100,00 mm
80,00 mm 90,00 mm

AISI 321 hexagon bars brightdrawn tolerance h11 DIN EN 10278 ( formerly DIN 176 ) long 3 mtr
Improved machinability
Sizes:

6,00 mm 15,00 mm 30,00 mm 60,00 mm
8,00 mm 16,00 mm 32,00 mm 65,00 mm
9,00 mm 17,00 mm 34,00 mm 70,00 mm
10,00 mm 18,00 mm 36,00 mm
11,00 mm 19,00 mm 41,00 mm
12,00 mm 22,00 mm 46,00 mm
13,00 mm 24,00 mm 50,00 mm
14,00 mm 27,00 mm 55,00 mm

AISI 321 round bar hotrolled / forged, peeled / turned acc. DIN EN 10060 ( formerly DIN 1013 ), long 4-6 mtr
Sizes:

Ø 20,00 mm Ø 42,00 mm Ø 90,00 mm Ø 145,00 mm Ø 210,00 mm Ø 310,00 mm Ø 525,00 mm
Ø 22,00 mm Ø 45,00 mm Ø 95,00 mm Ø 150,00 mm Ø 220,00 mm Ø 325,00 mm
Ø 24,00 mm Ø 50,00 mm Ø 100,00 mm Ø 155,00 mm Ø 230,00 mm Ø 340,00 mm
Ø 25,00 mm Ø 52,00 mm Ø 105,00 mm Ø 160,00 mm Ø 240,00 mm Ø 350,00 mm
Ø 28,00 mm Ø 55,00 mm Ø 110,00 mm Ø 165,00 mm Ø 250,00 mm Ø 360,00 mm
Ø 30,00 mm Ø 60,00 mm Ø 115,00 mm Ø 170,00 mm Ø 260,00 mm Ø 375,00 mm
Ø 32,00 mm Ø 65,00 mm Ø 120,00 mm Ø 175,00 mm Ø 270,00 mm Ø 400,00 mm
Ø 35,00 mm Ø 70,00 mm Ø 125,00 mm Ø 180,00 mm Ø 275,00 mm Ø 425,00 mm
Ø 36,00 mm Ø 75,00 mm Ø 130,00 mm Ø 185,00 mm Ø 280,00 mm Ø 450,00 mm
Ø 38,00 mm Ø 80,00 mm Ø 135,00 mm Ø 190,00 mm Ø 290,00 mm Ø 475,00 mm
Ø 40,00 mm Ø 85,00 mm Ø 140,00 mm Ø 200,00 mm Ø 300,00 mm Ø 500,00 mm

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x