manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

54SiCr6 Oil Hardened Spring Steel Wire Successful Delivered

We, Fushun Metal, had delivered a batch of oil hardened spring steel wire for Turkey client’s recently. The all goods passed inspection process and tested with several Item. Welcome send email to ask more details!

54sicr6 finished products-min

54sicr6 finished products-min

 

Introduce produce

54SiCr6(DIN) – Si-Cr heat treatable spring steel. Used for strained springs for cars and railway carriages and for surfaces requiring abrasion resistance. High strength, hardness and wear abrasion resistance. Low machinability, workability and weldability.

Client’s demand

Commodities Name
Quality Standard
Steel Grade
Diameter (mm)
Tolerance (mm)
Spring steel wire coil
EN 10270-2
54SiCr6
21
+/-0.1

1. Delivery Condition: Oil quenched+tempered.
2. Surface Condition: Black surface.
3.Tensile strength: 1400Mpa min.
4. Chemical composition:

C
Si
Mn
P max
S max
Cr
0.51-0.59
1.20-1.60
0.50-0.80
0.025
0.025
0.50-0.80

Quality inspection

Top quality, individualised services and direct proximity to the customer are just some of our strengths – in all key markets around the world. We offer our customers full support, from practice-oriented consulting all the way to a product ready for manufacturing, supplying top-quality, tailor-made solutions every step of the way.

Package and Delivery

Packed by plastic inside and woven or bag in the middle and then plastic outside to resist water and moisture. Wire shipments shall be suitable protected against mechanical damage or contamination during transport.

54sicr6 MTC-min

54sicr6 wire package-min

54sicr6 wire package-min

C
Si
Mn
P max
S max
Cr
0.51-0.59
1.20-1.60
0.50-0.80
0.025
0.025
0.50-0.80

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x