1.4547 Material to F44 Super Austenitic Stainless Steel is described as a 6% Mo super austenitic stainless
steel. The steel combines moderate mechanical strength (typically over 300 MPa yield strength) and high ductility with excellent corrosion resistance in seawater and a variety of industrial environments. Typically the alloy has a PREn(Pitting Resistance Equivalent) of 42-44 which ensures that the resistance to pitting corrosion is high. In addition, the steel provides good resistance to crevice corrosion.
Ambient and subzero temperature notch ductility is very good. These attributes mean that this high molybdenum stainless steel can be used successfully as an alternative to 300 series austenitic stainless steels (such as type 316) in applications where higher mechanical strength and/or
enhanced resistance to pitting and crevice corrosion is required. This alloy possesses a lower yield strength than that of duplex stainless steel (and much lower than that of super duplex steel) and pitting resistance which is comparable to super duplex stainless steel (such as UNS S32760 / S32750).

2 1.4547 Applications

F44 Super Austenitic Stainless Steel is ideally suited for use in halide environments and widely used in the chemical, marine, oil and gas industries. Typical applications include pumps, valves, heat exchangers, flanges and manifolds.

3 Quality Standard

ASTM A182 Standard Specification for Forged or Rolled Alloy-Steel Pipe Flanges, Forged Fittings, and Valves and Parts
EN 10088 part3 stainless steel

4 All Grades Comparison

ASTM A182 EN10088
F44 1.4547

 

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

5 +AT: Solution annealed

6 +P: Precipitation hardened

Suface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

5 1.4547 Chemical Composition(%)

Steel Grade C Si Mn P S Cr Ni Mo Cu N
F44 0.02 max 0.8 max 1.0 max 0.030 max 0.010 max 19.5-20.5 17.5-18.5 6.0-6.5 0.50-1.00 0.18-0.22
1.4547 0.02 max 0.7 max 1.0 max 0.030 max 0.010 max 19.5-20.5 17.50-18.50 6.0-7.0 0.50-1.00 0.18-0.25

6 Mechanical Properties (Annealed)

Hardness (HB) Tensile Strength (Mpa) Yield Strength (Mpa) Elongation (%) (Long.) Impact Value (J) (Long.)
260 max 650-850 300-340 35 min 100 min

7 Corrosion Resistance

: F44 Super Austenitic Stainless Steel offers higher resistance to abrasion, erosion and cavitation erosion than other austenitic stainless grades such as 316. F44 Super Austenitic Stainless Steel has excellent resistance to corrosion in sea water and concentrated halide environments, with good resistance to crevice corrosion in seawater.

8 Welding

:F44 Super Austenitic Stainless Steel is readily weldeable with welding procedures used for other austenitic stainless steel specifications. Welding should be carried out at the lowest heat possible as due to its austenite structure it can be prone to hot cracking.

9 Mill′s test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x