manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

28NiCrMoV8-5 DIN 1.6932 Alloy Structural Steels

28NiCrMoV8-5 DIN 1.6932 Alloy Structural Steels

28NiCrMoV8-5 DIN1.6932 Alloy Structural Steels

28NiCrMoV8-5 DIN1.6932 Alloy Structural Steels

1. 1.6932 Description

The alloy structural steels are provided with higher yield strength, tensile strength, endurance strength, yield ratio (about 0.85 generally ) enough plasticity and toughness.
The concentration of alloy element of this kind of steel is quite high, mainly are corrosion resistant steel, heat resistant steel, wear resistant steel, and other special steels of physical and chemical properties. Alloy structural steel has preferable mechanical property than that of carbon structural steel, high performance of heat treatment especially.

2. 1.6932 Application

The alloy structural steels are widely used in the filed of ship, vehicle, airplane, guided missile, weapons, railway, bridges, pressure vessel, machine tools, mechanical components with a bigger sectional size and so on.

3.All Grades Comparison

DIN EN
1.6932 28NiCrMoV8-5

4.Quality Standard

EN 10250 Open steel die forgings for general engineering purposes. Alloy special steels

5. 1.6932 Chemical Composition(%)

C Mn Si P S Cr Ni Mo V
0.24-0.32 0.15-0.40 0.40 max 0.035 max 0.035 max 1.00-1.50 1.80-2.10 0.35-0.55 0.05-0.15

6.Mechanical Properties(T=20°C if not differently stated) with Quenched and Tempered Delivery Condition

Diameter(mm) Tensile Strength Rm (Mpa) Yield Strength Rp0.2 (Mpa) Elongation A5 (%) Impact Value Kv (J) Room Temperature
160 max 800 min 630 min 14 min 45 min
160-330 750 min 590 min 15 min 40 min
330-660 750 min 590 min 15 min 40 min

7.HEAT TREATMENT:

  • Hardening Temperature:830oC-870oC
  • Tempering Temperature:550oC-850oC

8.Forging:

Hot forming temperature: 1050-850oC.

9.Mill′s test certificate:

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x