We, Fushun Metal, had delivered a batch of oil hardened spring steel wire for Turkey client’s recently. The all goods passed inspection process and tested with several Item. Welcome send email to ask more details!
Introduce produce
54SiCr6(DIN) – Si-Cr heat treatable spring steel. Used for strained springs for cars and railway carriages and for surfaces requiring abrasion resistance. High strength, hardness and wear abrasion resistance. Low machinability, workability and weldability.
Client’s demand
Commodities Name
|
Quality Standard
|
Steel Grade
|
Diameter (mm)
|
Tolerance (mm)
|
Spring steel wire coil
|
EN 10270-2
|
54SiCr6
|
21
|
+/-0.1
|
1. Delivery Condition: Oil quenched+tempered.
2. Surface Condition: Black surface.
3.Tensile strength: 1400Mpa min.
4. Chemical composition:
C
|
Si
|
Mn
|
P max
|
S max
|
Cr
|
0.51-0.59
|
1.20-1.60
|
0.50-0.80
|
0.025
|
0.025
|
0.50-0.80
|
Quality inspection
Top quality, individualised services and direct proximity to the customer are just some of our strengths – in all key markets around the world. We offer our customers full support, from practice-oriented consulting all the way to a product ready for manufacturing, supplying top-quality, tailor-made solutions every step of the way.
Package and Delivery
Packed by plastic inside and woven or bag in the middle and then plastic outside to resist water and moisture. Wire shipments shall be suitable protected against mechanical damage or contamination during transport.
C
|
Si
|
Mn
|
P max
|
S max
|
Cr
|
0.51-0.59
|
1.20-1.60
|
0.50-0.80
|
0.025
|
0.025
|
0.50-0.80
|