manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

1.4835 X9CrNiSiNCe21-11-2 Austenitic Heat Resisting Stainless Steel

1.4835 X9CrNiSiNCe21-11-2

1.4835 X9CrNiSiNCe21-11-2 Austenitic Heat Resisting Stainless Steel

1.4835 X9CrNiSiNCe21-11-2 Austenitic Heat Resisting Stainless Steel

The steel grade 1.4835 ( also called UNS S30815, 253MA and SS2368) is an austenitic stainless high temperature steel with good resistance to oxidation. The steel has been designed to be used at temperatures over 550°C, the most suitable temperature range is 850-1100°C. The steel suits for production of details with good resistance to temperature corrosion and relatively high strength at elevated temperatures. It also has good creep strength properties. 1.4835 is not magnetic but can be slightly magnetic after cold working or welding.

 

We offer steel grade 1.4835 in the following profiles

Steel grade1.4835 is a available as

machined round bar in dimensions 6 – 200 mm..

PLATE: 1-20mm thickness; 100-1500mm width

WIRE: 1-30mm diameter

STRIP: 0.5-4  thickness; 100-1219 mm width

Flat and SQUARE: 5-200 mm

If there is something you miss or wonder about you can always contact us to discuss your needs.

 

Typical application areas for 1.4835:

Ovens

Construction

Building

As details at high temperature

 

Good formability and weldability

1.4835 has a good weldability and can be welded with shielded metal arc welding, gas tungsten arc welding, plasma arc welding and submerged-arc welding. You shall use low heat input and use filler metals of type  EN 1.4835 when you weld. The steel can be both cold and hot formed but it can only be hardened by  cold working. The steel has high hardness and at machining you need to follow cutting recommendations.

 

Standard:

EN 10095: 1999 Heat Resisting Steels and Nickel Alloys

EN 10296-2: 2005 Welded circular steel tubes for mechanical and general engineering purposes. Stainless steel. Technical delivery conditions

EN 10297-2: 2005 Seamless circular steel tubes for mechanical and general engineering purposes. Stainless steel. Technical delivery conditions

EN 10088-1: 2005 Stainless steels. List of stainless steels

 

Equivalent grades of X9CrNiSiNCe21-11-2 (1.4835)

EU/EN :X9CrNiSiNCe21-11-2

USA / UNS : S30815

Sweden SS : 2368

Inter ISO : X7CrNiSiNCe21-11

 

Chemical composition % of X9CrNiSiNCe21-11-2 (1.4835)

 

C Si Mn Ni P S Cr Ce N
0.05 – 0.12 1.4 – 2.5 max   1 44481 max   0.045 max   0.015 20 – 22 0.03 – 0.08 0.12 – 0.2

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com