manufacturer of tool steel, stainless steel, nickel alloy, alloy steel

1.4313 X3CrNiMo13-4 Martensitic Stainless Steel

1.4313 X3CrNiMo13-4 Martensitic Stainless Steel

1.4313 X3CrNiMo13-4 Martensitic Stainless Steel

Introduce

1.4313 Stainless steel is a martensitic stainless steel grade, which can be hardened with heat threatment. This grade is written as 1.4313 or X3CrNiMo13-4 according to EN norm and it is written as UNS S41500 according to UNS norm. It starts with 415 number according to UNS norm so because of this, some sources accept this grade also as AISI 415 stainless steel. 1.4313 material is a magnetic grade and 1.4313 heat treated according to the following three different heat thereatment contitions: QT650, QT780, QT900. The numbers 650, 780 and 900 are showing the minimum tensile MPA strenght of the materials.

Our supply size:

Diameter : 80 to 600 mm ;

Length : 1000 to 9000 mm ;

 

Our advantage:

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

Equivalent grades of steel X3CrNiMo13-4 (1.4313)

EU USA France Sweden
EN AFNOR SS
X3CrNiMo13-4 S41500 Z6CN13-04 2385

 

Chemical composition % of steel X3CrNiMo13-4 (1.4313): EN 10088-2-2005

C Si Mn Ni P S Cr Mo N
max 0.05 max 0.7 max 1.5 3.5 – 4.5 max 0.04 max 0.015 12-114 0.3 – 0.7 max 0.02

 

Mechanical properties of steel X3CrNiMo13-4 (1.4313)

Rm – Tensile strength (MPa) (+A) 1100
Rm – Tensile strength (MPa) (+QT650) 700-800
Rm – Tensile strength (MPa) (+QT780) 780-980
Rm – Tensile strength (MPa) (+QT900) 900-1100
Rp0.2 0.2% proof strength (MPa) (+QT650) 520
Rp0.2 0.2% proof strength (MPa) (+QT780) 620
Rp0.2 0.2% proof strength (MPa) (+QT900) 800

 

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mill test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

 

We also supply :

1.2510/H10, 1.2842, 1.2379/D2, 1.2080/X210Cr12/D3, 1.2436, 1.2365, 1.2885, 1.2343, 1.2344/H13/SKD61, 1.2581/H21, 1.2709, 1.2345, 1.2738/P20NI, 1.2083/420J2, 1.2316, 1.2312/P20S, 1.23111.2764

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x