1.4021 X20Cr13 Stainless Steel

1.4021 X20Cr13 Stainless Steel

1.4021 X20Cr13 Stainless Steel

Grade :X20Cr13

Number:1.4021

Classification:Martensitic stainless steel

Density:7.7 g/cm³

 

We offer steel grade 1.4021 in the following profiles

Steel grade 1.4021 is available as machined round bar in the dimensions 5 – 600 mm.

If there is something you miss or wonder about you can always contact us to discuss your needs.

 

Our advantage :

  1. High Quality, Reasonable Price
  2. Over 40 Years Experience
  3. ISO NQA Certificated Factory
  4. Worldwide shipping
  5. Emergency Orders and Fast Delivery

 

Standard:

EN 10088-2: 2005 Stainless steels. sheet/plate and strip of corrosion resisting steels for general purposes

EN 10088-3: 2005 Stainless steels. semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels

EN 10151: 2003 Stainless steel strip for springs. Technical delivery conditions

EN 10250-4: 2000 Open steel die forgings for general engineering purposes. Stainless steels

EN 10088-1: 2005 Stainless steels. List of stainless steels

EN 10088-5: 2009 Stainless steels. bars, rods, wire, sections and bright products of corrosion resisting steels

EN 10088-4: 2009 Stainless steels. sheet/plate and strip of corrosion resisting steels

 

Chemical composition % of steel X20Cr13 (1.4021): EN 10088-2-2005

C Si Mn P S Cr
0.16 – 0.25 max 1 max 1.5 max 0.04 max 0.015 12-14

 

Equivalent grades of steel X20Cr13 (1.4021)

EU USA Germany Japan France England China Czechia Russia
EN DIN,WNr JIS AFNOR BS GB CSN GOST
X20Cr13 420 X20Cr13 SUS420J1 X20Cr13 420S29 2Cr13 17022 20KH13
  S42010     Z20C13 420S37 X20Cr13    

 

The steel grade 1.4021(also called ASTM 420 and SS2303) is a high tensile strength martensitic stainless steel with good corrosion properties. The steel is machinable and suits good for production of details with good resistance to e.g. air water steam, freshwater, certain alkaline solutions and other mildly aggressive chemicals.  It shall not be used in marine or in chloride environment. The steel is magnetic and in the quenched and tempered condition.

 

Application

Some typical application areas for EN 1.4021:

Pump- and Valve parts

Shafting

Spindels

Piston rods

Fittings

Stirrers

Bolts

Nuts

 

Weldable steel for for machining

1.4021 is possible to weld and shall be welded with welding consumables similar to that of the parent one. The steel is generally easier to machine than ”conventional” austenitic steels. The heat treatment condition of 1.4021 is QT 700 and it should be hot formed in the temperature range 1100-800°C. Slow cooling after hot forming.

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

We also supply :

1.2510/H10, 1.2842, 1.2379/D2, 1.2080/X210Cr12/D3, 1.2436, 1.2365, 1.2885, 1.2343, 1.2344/H13/SKD61, 1.2581/H21, 1.2709, 1.2345, 1.2738/P20NI, 1.2083/420J2, 1.2316, 1.2312/P20S, 1.23111.2764

For all products, please check here: Fushun products

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Fushun TEL: +86-731-89903933

Fushun FAX: +86-731-89853933

General Manager: Ms. Florence Tang

Whatsapp/Phone/WeChat:+86-13319591838

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

Whatsapp:+86-18692275455

x